Dry sliding wear behavior of TIG welding clad WC composite coatings

dc.contributor.authorBuytoz, S
dc.contributor.authorUlutan, M
dc.contributor.authorYildirim, MM
dc.date.accessioned2026-08-12T17:43:44Z
dc.date.issued2005
dc.departmentFırat Üniversitesi
dc.description.abstractIn this study, melted tungsten carbide powders on the surface of AISI 4340 steel was applied by using tungsten inert gas (TIG) method. It was observed that it has been solidified in different microstructures depending on the production parameters. As a result of microstructure examinations, in the surface modified layers an eutectic and dendrite solidification was observed together with WC, W2C phases. In the layer produced, the hardness values varied between 950 and 1200 HV. The minimum mass loss was observed in the sample, which was treated in 1.209 mm/s production rate, 0.5 g/s powder feed rate and 13.9 kJ/cm heat input. (c) 2005 Elsevier B.V All rights reserved.
dc.identifier.doi10.1016/j.apsusc.2005.02.088
dc.identifier.endpage1323
dc.identifier.issn0169-4332
dc.identifier.issn1873-5584
dc.identifier.issue5
dc.identifier.orcid0000-0003-1821-6486
dc.identifier.scopus2-s2.0-27944474823
dc.identifier.scopusqualityQ1
dc.identifier.startpage1313
dc.identifier.urihttps://doi.org/10.1016/j.apsusc.2005.02.088
dc.identifier.urihttps://hdl.handle.net/11508/60254
dc.identifier.volume252
dc.identifier.wosWOS:000233985900016
dc.identifier.wosqualityQ1
dc.indekslendigikaynakWeb of Science
dc.indekslendigikaynakScopus
dc.language.isoen
dc.publisherElsevier
dc.relation.ispartofApplied Surface Science
dc.relation.publicationcategoryMakale - Uluslararası Hakemli Dergi - Kurum Öğretim Elemanı
dc.rightsinfo:eu-repo/semantics/closedAccess
dc.snmzKA_WoS_20260511
dc.subjectTIG method
dc.subjectsurface modification
dc.subjectabrasive wear
dc.subjectdendrite
dc.subjectWC
dc.subjectM7C3
dc.titleDry sliding wear behavior of TIG welding clad WC composite coatings
dc.typeArticle