Determination of the Cracking Resistance of Hot-Mix Asphalt Prepared with Capsules Containing Waste Oil

dc.contributor.authorOzdemir, Ahmet Munir
dc.contributor.authorYalcin, Erkut
dc.contributor.authorYilmaz, Mehmet
dc.contributor.authorKok, B. Vural
dc.contributor.authorHernandez, Alvaro Garcia
dc.date.accessioned2026-08-12T17:39:04Z
dc.date.issued2024
dc.departmentFırat Üniversitesi
dc.description.abstractHot-mix asphalts are composite materials with self-healing properties: cracks in pavements constructed with these asphalts can close without external help. However, this self-healing process is slow, and cracks may reopen quickly. To increase the self-healing ratio and accelerate the healing process, capsules containing two different types of waste oil (vegetable and mineral oil) were added to the mixture at four different proportions (0.25%, 0.50%, 0.75%, and 1.00% by weight of the mixture). This research evaluated the effect of the capsule addition on the strength of the mixture against cracking. Experiments using samples with added semicircular capsules and samples containing no added capsules were carried out according to the linear elastic and elastic-plastic fracture mechanical principles. The self-healing properties of the hot-mix asphalt were determined. The results showed that the highest strength against cracking at low temperature was found in the sample with a proportion of 0.25% capsules of both types (waste vegetable and mineral oil). In addition, the oil released from the capsules increased the self-healing properties of the hot-mix asphalt. Samples fractured at 0 degrees C had better healing than the samples fractured at 25 degrees C.
dc.description.sponsorshipScientific and Technological Research Council of Turkey (TUBITAK); TUBITAK [217M570]
dc.description.sponsorshipThis study was carried out within the scope of the Scientific and Technological Research Council of Turkey (TUBITAK). The authors gratefully acknowledge the financial support provided by TUBITAK to Research project 217M570.
dc.identifier.doi10.1061/JPEODX.PVENG-1315
dc.identifier.issn2573-5438
dc.identifier.issue4
dc.identifier.orcid0000-0002-6389-4211
dc.identifier.orcid0000-0002-4872-154X
dc.identifier.orcid0000-0001-8730-6632
dc.identifier.orcid0000-0002-7496-6006
dc.identifier.scopus2-s2.0-85199451796
dc.identifier.scopusqualityQ2
dc.identifier.urihttps://doi.org/10.1061/JPEODX.PVENG-1315
dc.identifier.urihttps://hdl.handle.net/11508/58688
dc.identifier.volume150
dc.identifier.wosWOS:001338181700007
dc.identifier.wosqualityQ2
dc.indekslendigikaynakWeb of Science
dc.indekslendigikaynakScopus
dc.language.isoen
dc.publisherAsce-Amer Soc Civil Engineers
dc.relation.ispartofJournal of Transportation Engineering Part B-Pavements
dc.relation.publicationcategoryMakale - Uluslararası Hakemli Dergi - Kurum Öğretim Elemanı
dc.rightsinfo:eu-repo/semantics/closedAccess
dc.snmzKA_WoS_20260511
dc.subjectSelf-healing
dc.subjectAsphalt mixture
dc.subjectCalcium alginate capsules
dc.subjectWaste vegetable oil
dc.subjectWaste mineral oil
dc.titleDetermination of the Cracking Resistance of Hot-Mix Asphalt Prepared with Capsules Containing Waste Oil