Wear behavior of TiB2 inoculated 20Cr-3Mo-4C high chromium white cast irons

dc.contributor.authorYilmaz, Serdar Osman
dc.date.accessioned2026-08-12T17:29:42Z
dc.date.issued2007
dc.departmentFırat Üniversitesi
dc.description.abstractFeTi, B2O3, Al, and FeW particulates, approximately 40-60 mu m in size, were mixed in stoichiometric ratio and sintered at 1,200 degrees C. The sintered particulates were added as 5 wt% to molten high chromium white cast iron over 50 C-deg above the melting temperature, and stirred at 1,000 rpm. The samples were investigated in three groups: (1) high Cr white cast iron inoculated by the particulates sintered from Al-FeTi-B2O3 particulates; (2) high Cr white cast iron inoculated by the sintered particulates derived from Al-FeTi, B2O3, and FeW particulates; and (3) specimens of the second group that were subsequently homogenized. The microhardness of ceramic particulates was measured as 2,800-3,400 HV10. The effect of sintered particulate volume fraction on the abrasive wear resistance of the high chromium white cast iron was determined. The wear resistance and hardness of the composites improved significantly as a result of particulate inoculation. The application of the homogenization heat treatment to the inoculated samples produced a microstructure having homogeneously distributed particulates.
dc.identifier.doi10.1007/s10853-006-1430-8
dc.identifier.endpage6778
dc.identifier.issn0022-2461
dc.identifier.issue16
dc.identifier.scopus2-s2.0-34547288218
dc.identifier.scopusqualityQ1
dc.identifier.startpage6769
dc.identifier.urihttps://doi.org/10.1007/s10853-006-1430-8
dc.identifier.urihttps://hdl.handle.net/11508/55808
dc.identifier.volume42
dc.identifier.wosWOS:000247934700041
dc.identifier.wosqualityQ2
dc.indekslendigikaynakWeb of Science
dc.indekslendigikaynakScopus
dc.language.isoen
dc.publisherSpringer
dc.relation.ispartofJournal of Materials Science
dc.relation.publicationcategoryMakale - Uluslararası Hakemli Dergi - Kurum Öğretim Elemanı
dc.rightsinfo:eu-repo/semantics/closedAccess
dc.snmzKA_WoS_20260511
dc.subjectMetal-Matrix Composites
dc.subjectAbrasion Resistance
dc.subjectAlloys
dc.subjectMorphology
dc.subjectCarbides
dc.subjectFracture
dc.titleWear behavior of TiB2 inoculated 20Cr-3Mo-4C high chromium white cast irons
dc.typeArticle

Dosyalar