Oxidation of high-temperature Cu-Al-Fe shape memory alloy
| dc.contributor.author | Yildiz, Koksal | |
| dc.date.accessioned | 2026-08-12T17:32:42Z | |
| dc.date.issued | 2016 | |
| dc.department | Fırat Üniversitesi | |
| dc.description.abstract | Isothermal oxidation behavior of the high-temperature Cu-13Al-5Fe (in mass, %) SMA on temperature range of 500-900 A degrees C was studied using thermo-gravimetric method. TG curve showed that the alloy has linear oxidation characteristics. From thermo-gravimetric measurements, it was determined that the alloy shows abnormal oxidation characteristics at 600 A degrees C. As K (P) values of the alloy at oxidation temperatures of 700 and 800 A degrees C were calculated as 0.00166 mg cm(-2) s(-1) and 0.0022 mg cm(-2) s(-1), respectively, K (P) value at 600 A degrees C was found as 0.0029 mg cm(-2) s(-1). DTA curve exhibited that reason of the abnormal oxidation behavior at 600 A degrees C is the endothermic reaction which causes dissolution of Fe(Al,Cu) precipitates within matrix at 568.13 A degrees C. XRD patterns of the oxidized samples were found to be compatible with the results obtained from thermo-gravimetric measurements. | |
| dc.identifier.doi | 10.1007/s10973-015-4912-6 | |
| dc.identifier.endpage | 412 | |
| dc.identifier.issn | 1388-6150 | |
| dc.identifier.issn | 1572-8943 | |
| dc.identifier.issue | 1 | |
| dc.identifier.orcid | 0000-0002-3484-4653 | |
| dc.identifier.scopus | 2-s2.0-84953439641 | |
| dc.identifier.scopusquality | Q1 | |
| dc.identifier.startpage | 409 | |
| dc.identifier.uri | https://doi.org/10.1007/s10973-015-4912-6 | |
| dc.identifier.uri | https://hdl.handle.net/11508/56744 | |
| dc.identifier.volume | 123 | |
| dc.identifier.wos | WOS:000368187700039 | |
| dc.identifier.wosquality | Q2 | |
| dc.indekslendigikaynak | Web of Science | |
| dc.indekslendigikaynak | Scopus | |
| dc.language.iso | en | |
| dc.publisher | Springer | |
| dc.relation.ispartof | Journal of Thermal Analysis and Calorimetry | |
| dc.relation.publicationcategory | Makale - Uluslararası Hakemli Dergi - Kurum Öğretim Elemanı | |
| dc.rights | info:eu-repo/semantics/closedAccess | |
| dc.snmz | KA_WoS_20260511 | |
| dc.subject | Cu-Al-Fe | |
| dc.subject | Oxidation | |
| dc.subject | High-temperature SMA | |
| dc.subject | TG/DTA | |
| dc.title | Oxidation of high-temperature Cu-Al-Fe shape memory alloy | |
| dc.type | Article |