DETERMINATION OF POLYSTYRENE-HYDROCARBON INTERACTION PARAMETERS AND SOLUBILITY PARAMETER USING INVERSE GAS-CHROMATOGRAPHY
| dc.contributor.author | OZDEMIR, E | |
| dc.contributor.author | ACIKSES, A | |
| dc.contributor.author | COSKUN, M | |
| dc.date.accessioned | 2026-08-12T17:10:20Z | |
| dc.date.issued | 1992 | |
| dc.department | Fırat Üniversitesi | |
| dc.description.abstract | The weight fraction activity coefficients (a1/w1)infinity and Flory - Huggins X parameters have been determined by using inverse gas chromatography technique over the temperature range of 433-453 K for four hydrocarbons on polystyrene. The Hildebrand solubility parameter delta-2 of polystyrene was then calculated. The values of delta-2 obtained from DELTA-G1BAR infinity and X parameters were found to agree with literature data. | |
| dc.identifier.doi | 10.1080/10101329208054565 | |
| dc.identifier.endpage | 70 | |
| dc.identifier.issn | 1060-1325 | |
| dc.identifier.scopus | 2-s2.0-0026992499 | |
| dc.identifier.scopusquality | Q2 | |
| dc.identifier.startpage | 63 | |
| dc.identifier.uri | https://doi.org/10.1080/10101329208054565 | |
| dc.identifier.uri | https://hdl.handle.net/11508/50687 | |
| dc.identifier.volume | 29 | |
| dc.identifier.wos | WOS:A1992HK47900008 | |
| dc.identifier.wosquality | Q3 | |
| dc.indekslendigikaynak | Web of Science | |
| dc.indekslendigikaynak | Scopus | |
| dc.language.iso | en | |
| dc.publisher | Marcel Dekker Inc | |
| dc.relation.ispartof | Journal of Macromolecular Science-Pure and Applied Chemistry | |
| dc.relation.publicationcategory | Makale - Uluslararası Hakemli Dergi - Kurum Öğretim Elemanı | |
| dc.rights | info:eu-repo/semantics/closedAccess | |
| dc.snmz | KA_WoS_20260511 | |
| dc.subject | Polymer | |
| dc.title | DETERMINATION OF POLYSTYRENE-HYDROCARBON INTERACTION PARAMETERS AND SOLUBILITY PARAMETER USING INVERSE GAS-CHROMATOGRAPHY | |
| dc.type | Article |