Electrical conductivity and electrical modulus properties of 13SrO-5.5Fe2O3-O.5Al2O3-8B2O3 magnetic glass ceramic

dc.contributor.authorYakuphanoğlu, Fahrettin
dc.contributor.authorZaitsev, D. D.
dc.contributor.authorTrusov, L. A.
dc.contributor.authorKazin, P. E.
dc.date.accessioned2026-08-12T17:29:38Z
dc.date.issued2007
dc.departmentFırat Üniversitesi
dc.description.abstractThe direct and alternating current conductivity and electrical modulus properties of 13SrO-5.5Fe(2)O(3)-0.5Al(2)O(3)-8B(2)O(3) magnetic glass ceramic have been investigated by complex impedance spectroscopy and direct current conductivity techniques. The direct current conductivity results indicate that 13SrO-5.5Fe(2)O3-0.5Al(2)O(3)-8B(2)O(3) magnetic glass ceramic exhibits an oxide semiconductor behavior with activation energy (Delta E = 0.37 eV) and conductivity at room temperature (sigma(25) = 2.97 x 10(-8)S/cm) values and a thermally activated process conductivity mechanism. Alternating conductivity results suggest that the correlated barrier hopping conductivity is dominant in alternating current conductivity mechanism of the sample. The dielectric constant values of SrO-Al2O3-Fe2O3-B2O3 magnetic glass ceramic increase with increasing temperature. The imaginary part of the modulus at different temperatures shows a relaxation peak and its position shifts to higher frequency with increasing temperature. This suggests a temperature-dependent relaxation. The activation energy of the relaxation process and relaxation time at infinite temperature were found to be 0.26 eV and 3.29 x 10(-8) s, respectively. (C) 2006 Elsevier B.V. All rights reserved.
dc.identifier.doi10.1016/j.jmmm.2006.09.006
dc.identifier.endpage47
dc.identifier.issn0304-8853
dc.identifier.issn1873-4766
dc.identifier.issue1
dc.identifier.orcid0000-0002-1415-2190
dc.identifier.scopus2-s2.0-33947159606
dc.identifier.scopusqualityQ2
dc.identifier.startpage43
dc.identifier.urihttps://doi.org/10.1016/j.jmmm.2006.09.006
dc.identifier.urihttps://hdl.handle.net/11508/55766
dc.identifier.volume312
dc.identifier.wosWOS:000245793800010
dc.identifier.wosqualityQ2
dc.indekslendigikaynakWeb of Science
dc.indekslendigikaynakScopus
dc.language.isoen
dc.publisherElsevier
dc.relation.ispartofJournal of Magnetism and Magnetic Materials
dc.relation.publicationcategoryMakale - Uluslararası Hakemli Dergi - Kurum Öğretim Elemanı
dc.rightsinfo:eu-repo/semantics/closedAccess
dc.snmzKA_WoS_20260511
dc.subjectoxide
dc.subjectmagnetic semiconductor
dc.subjectelectrical conductivity
dc.subjectglass ceramics
dc.subjectstrontium hexaferrite
dc.titleElectrical conductivity and electrical modulus properties of 13SrO-5.5Fe2O3-O.5Al2O3-8B2O3 magnetic glass ceramic
dc.typeArticle

Dosyalar